HfO2 films were produced from Hf[N(CH3)(C2H5)]4 and H2O, on borosilicate glass, indium-tin-oxide (ITO), and Si(100) substrates, in the temperature range 150–325 °C, using atomic layer deposition (ALD). In the temperature range 200–250 °C, the growth rate of the HfO2 films was 0.09 nm per cycle, but increased with both increasing and decreasing temperatures. The self-limiting adsorption of Hf[N(CH3)(C2H5)]4 at 250 °C was verified. The films were stoichiometric dioxides with an O/Hf ratio of 2.0 ± 0.1. The concentrations of residual carbon, nitrogen, and hydrogen, determined using ion beam analysis, were 0.3–0.6 at.-%, 0.1–0.2 at.-%, and 2–3 at.-%, respectively. The films crystallized at growth temperatures exceeding 150–175 °C, and consisted mainly of the monoclinic HfO2 phase. The refractive index of the films varied between 2.08 and 2.10. The effective permittivities of the HfO2 films grown in the temperature range 200–300 °C varied between 11 and 14.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Kukli et al. (2002) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: