Herein, a facile method to fabricate high-performance Ag 2 Se 1– x S x thermoelectric (TE) films on nylon membranes was developed. The Ag 2 Se 1– x S x TE films were fabricated by first wet-chemically synthesizing Ag 2 Se 1– x S x powders beginning from Se/Ag 2 S molar ratios of 0.5, 0.6, 0.7, 0.8, and 0.9, followed by vacuum-assisted filtration of the powders on nylon membranes, and finally by hot-pressing. When the Se/Ag 2 S molar ratio is ≤0.7, the films prepared consist of Se-substituted Ag 2 S with a monoclinic structure; when it is 0.8, the film obtained is composed of Ag 2 S and Ag 2 Se in two phases; when it is 0.9, the film prepared consists of S-substituted Ag 2 Se with an orthorhombic structure. The S-substituted Ag 2 Se film exhibits a power factor of ∼1035.4 μW m –1 K –2 at 300 K and excellent flexibility (it retains 94.4% of the pristine electrical conductivity after being bended 1000 times around a rod with a diameter of 8 mm). Furthermore, a flexible TE generator consisting of six legs was assembled with the S-substituted Ag 2 Se film, and it produces a maximum output power of ∼ 5.29 μW (equivalent to a power density of ∼10.5 W m –2 ) under a temperature gradient of 28.6 K. This work provides an avenue to explore high-performance and low-cost flexible TE devices for room temperature use.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: