This is the authors' abstract. We don't add key points for this paper.
Junctions with Al2O3 and AIN barriers were fabricated through contact shadow masks (0.25mm2-size) and by a self-aligned lithography process (9×2μm2-size). The Al2O3 barrier was formed by plasma oxidation. The AlN barrier was prepared by dc reactive magnetron sputtering. Room temperature tunneling magnetoresistance (TMR) is 1.6% for the AIN junctions and up to 24% for the Al2O3 junctions. The TMR for all junctions decreases with increase of applied bias voltage and drops to half its initial value at a bias voltage between 116 mV and 437 mV. The weakest bias voltage dependence occurs for junctions with higher barrier heights, and thinner barrier thickness. Annealing at 100-200 °C leads to a 20% increase of TMR and a 40% decrease of junction resistance for the 9×2μm2 junctions, leading to a maximum TMR of 27%. Both TMR and junction resistance were increased for the AlN junctions due to annealing.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Sun et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: