Answers are grounded in this paper and cite their sources.
Three procedures to obtain bone inductive implants were tested heterotopically in 3-month-old allogeneic rats: 1) antigen-extracted HCl-decalcified at 4 degrees C, autolysed implant (AAA bone); 2) HCl-decalcified implant at 4 degrees C; 3) HCl-decalcified implant at room temperature. Each type of implant was either deep-frozen at -35 degrees C for at least 2 months or immediately freeze-dried. The bone inductive capacity of the differently HCl-decalcified cortical bone implant was evaluated at 2 months by isotopic strontium incorporation and by ash-weight measurements. Bone HCl-decalcification alone, either at 4 degrees C or at room temperature, gave a higher new bone yield than the freeze-dried AAA bone. The type or short-term preservation technique had no effect on the osteoinductive capacity of either of the differently treated implants, AAA bone expected.
No takes yet. Share an insight, caveat, or question.
Delloye et al. (1985) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: