Highly efficient HPW(x)/MIL-100(Fe) catalysts with different phosphotungstic acid (HPW) loading (x, wt%) were successfully synthesized by a one-step hydrothermal method and characterized by XRD, SEM, FTIR, and BET. The influences of HPW loading, catalyst dosage, temperature, and O/S molar ratio on oxidative desulfurization (ODS) were investigated. The results indicated that the HPW(x)/MIL-100(Fe) retained the structure of its parent MIL-100(Fe). The MIL-100(Fe) presented a high surface area, which is beneficial to dispersion of HPW. The HPW(x)/MIL-100(Fe) with HPW loading of 40% exhibited excellent ODS activity. At a temperature of 50 °C, a catalyst dosage of 0.06 g, and an O/S molar ratio of 4, 100% desulfurization was achieved within 90 min for benzothiophene, dibenzothiophene, and 4,6-dimethyl-dibenzothiophene. The high catalytic activity of HPW(x)/MIL-100(Fe) can be attributed to highly dispersed HPW active sites with a high specific surface area.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: