Sintering ceramic/ceramic composites is difficult if the constituents have widely different sintering rates. The differential sets up internal, tensile hydrostatic stress. This stress retards the shrinkage of the composite. In addition, the tensile components of internal stresses can potentially generate flaws. Analysis has shown that the magnitude of the tensile stresses is about equal to the sintering pressure. Therefore, densification under a superimposed pressure, about two to five times the sintering pressure, should lead to full density and eliminate processing flaws. Since the sintering pressure has been measured to be {approx} 1 MPa in several studies, it is likely that low-pressure, hot isostatic pressing can be used to produce dense and reliable ceramic/ceramic composites. Experimental results on a model system, which support the above hypothesis, are presented.
No takes yet. Share an insight, caveat, or question.
Bordia et al. (1988) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: