Spectroscopic analysis demonstrates the transformation pathways of metakaolinite into zeolite Na-A, indicating that precursor condensation precedes solid-state rearrangement.
29 Si and 27Al NMR, XRD, IR, SEM and EDAX have been used to examine the synthesis of zeolite Na-A from metakaolinite. When metakaolinite is treated with 5 mol dm–3 NaOH, five- and six-coordinated Al in the aluminous matrix is rapidly converted into four-coordination. The siliceous matrix of kaolinite is partially preserved in metakaolinite and is responsible for the residual long-range order in the ab plane. The siliceous matrix is much more stable to the base than the aluminous matrix. 27Al NMR spectra recorded with fast MAS (> 12 kHz) allow quantification of Al and show that metakaolinite is most reactive after treatment at ca. 700 °C, when the populations of four- and five-coordinated Al are at a maximum and the population of six-coordinated Al at a minimum. Upon treatment with alkali, metakaolinite slowly dissolves. SiO4+4 and Al(OH)4–4 ions in solution condense to an amorphous phase with Si/Al = 1. This direct precursor transforms into zeolite A by a solid-state rearrangement.
No takes yet. Share an insight, caveat, or question.
Klinowski et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: