Ultraviolet light emitting diodes (LEDs) have been grown using metalorganic vapor phase epitaxy, while monitoring the 550 nm reflected light intensity. During nucleation of GaN on sapphire, the transition from three-dimensional (3D) grain growth to two-dimensional (2D) coalesced growth was intentionally delayed in time by lowering the NH3 flow during the initial high temperature growth. Initially, when the reflectance signal is near zero, the GaN film is rough and composed of partly coalesced 3D grains. Eventually, the reflected light intensity recovers as the 2D morphology evolves. For 380 nm LEDs grown on 3D nucleation layers, we observe increased light output. For LEDs fabricated on GaN films with a longer recovery time an output power of 1.3 mW at 20 mA current was achieved.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Koleske et al. (2002) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: