Answers are grounded in this paper and cite their sources.
Transition metal (TM) Mn 2+ activated Ca--SiAlON phosphors with compositions of Ca1x Si 9 Al 3 ON 15 :xMn 2+ (x=0.020.16) have been designed and synthesized through a high temperature solid-state reaction. In the polyhedron structure of Ca--SiAlON host (P31c), Mn 2+ ions can be accommodated in the lattice without destabalizing the crystal structure, which has been revealed by both XRD and neutron powder diffraction (NPD) characterization. The successful doping of TM Mn 2+ in host was further confirmed by magnetic susceptibility characterization and the occupation of Mn 2+ in lattice was analyzed through Rietveld refinement of crystal structure. The slight left-shift of diffraction peaks in XRD patterns and Gaussian fitting sub-bands of emission spectra all proved that the activators Mn 2+ in Ca--SiAlON host not only incorporate into the "separated interstitial sites", but also modestly substitute for Al 3+ sites. The phosphors mainly deliver orange-red emission centered at 600nm under UV excitation, which is ascribed to the typical characteristic 4 T 1 ( 4 G) 6 A 1 ( 6 S) electron transition of divalent Mn 2+. The highest photoluminescence (PL) intensity arrives at x=0.12 of Mn 2+ doping concentration in compositions, then the doping concentration quenching occurs. In addition, through calculating the critical transfer distance, it indicates that the dipole-quadrupole (d-q) interaction is the major mechanism for doping concentration quenching in the phosphors. With the increment of Mn 2+ content up to x=0.12 (quenching concentration), the decay time decreases monotonically from 7.5 to 5.5s, ascribed to the non-radiative energy migration among Mn 2+ ions in the phosphors.
No takes yet. Share an insight, caveat, or question.
Liu Q (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: