The ϵ‐Fe 2 O 3 phase is commonly considered an intermediate phase during thermal treatment of maghemite (γ‐Fe 2 O 3 ) to hematite (α‐Fe 2 O 3 ). The routine method of synthesis for ϵ‐Fe 2 O 3 crystals uses γ‐Fe 2 O 3 as the source material and requires dispersion of γ‐Fe 2 O 3 into silica, and the obtained ϵ‐Fe 2 O 3 particle size is rather limited, typically under 200 nm. In this paper, by using a pulsed laser deposition method and Fe 3 O 4 powder as a source material, the synthesis of not only one‐dimensional Fe 3 O 4 nanowires but also high‐yield ϵ‐Fe 2 O 3 nanowires is reported for the first time. A detailed transmission electron microscopy (TEM) study shows that the nanowires of pure magnetite grow along [111] and <211> directions, although some stacking faults and twins exist. However, magnetite nanowires growing along the <110> direction are found in every instance to accompany a new phase, ϵ‐Fe 2 O 3 , with some micrometer‐sized wires even fully transferring to ϵ‐Fe 2 O 3 along the fixed structural orientation relationship, (001) ∥ (111) , [010] ∥ <110> . Contrary to generally accepted ideas regarding epsilon phase formation, there is no indication of γ‐Fe 2 O 3 formation during the synthesis process; the phase transition may be described as being from Fe 3 O 4 to ϵ‐Fe 2 O 3 , then to α‐Fe 2 O 3 . The detailed structural evolution process has been revealed by using TEM. 120° rotation domain boundaries and antiphase boundaries are also frequently observed in the ϵ‐Fe 2 O 3 nanowires. The observed ϵ‐Fe 2 O 3 is fundamentally important for understanding the magnetic properties of the nanowires.
No takes yet. Share an insight, caveat, or question.
Ding et al. (2007) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: