Answers are grounded in this paper and cite their sources.
The formation of ncl-Si in the amorphous matrix a-SiOx:H using a time-modulated DC plasma at an elevated oxygen content of C_O₂ = 21.5 mol % in a gas mixture of (SiH4–Ar–O2) is investigated. Plasma modulation implies the repeated (n = 180) switching on (for ton = 5, 10, 15 s) and switching off (for toff = 5, 10, 15 s) of the magnet coil of the DC magnetron. The effect of self-induction is used to enhance the processes of SiH4 dissociation, the formation of Si nanoparticles, and the ionization of oxygen and ncl-Si flows towards the electrodes. The samples are located both on an electrically isolated substrate holder near the anode and on the cathode (beyond its erosion zone). These experiments show that the shape of the dependences of the photoluminescence intensity I_PL^ncl - Si on the wavelength Λ are identical for all pairs of samples on the anode and cathode. When the ton value is small (ton = 5 s), the difference in the sample location only slightly affects the infrared (IR) spectra. At longer times ton (≥10 s) and a short time toff (5 s), the amorphous matrix located on the cathode is enriched with oxygen (as compared with that near the anode). The optimal plasma-modulation parameters are found to be toff/ton = 5, 10, 15/10 and toff/ton = 5, 10/15; under these conditions, the amorphous matrix has a “perfect structure” and is transparent to radiation, and the I_PL^ncl - Si value is the largest in the range λ ≈ 0.75–0.9 μm.
No takes yet. Share an insight, caveat, or question.
Undalov et al. (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: