This is the authors' abstract. We don't add key points for this paper.
Narrowband optical filters were made by direct deposition of thin films of TiO/sub 2/ and SiO/sub 2/ on the ends of optical fibers. Single-cavity etalons with bandwidths of 1.1 nm, insertion loss of 1 dB, and 2.25 nm, insertion loss of 0.5 dB, were made. It is necessary to use fibers with mode fields larger than standard single mode fiber. Thermal expansion was used to diffuse the core dopant and produce tapered-core fibers with mode-field diameters of 22 mu m.>
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Stone et al. (1992) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: