First-principles calculations of the energetics of the In-terminated GaN(0001), $(0001̱),$ $(101̱1),$ and (1011) surfaces indicate that In has a substantial effect on the relative energies of formation of these surfaces. Indium-induced changes in the surface energetics enable the formation of inverted hexagonal pyramid defects having $(101̱1)$ facets at the termination of threading defects on the (0001) surface of pseudomorphic InₓGa_1-xN films. For dislocations terminating on the InₓGa_1-xN(0001̱) surface, the calculations predict that large (1011) faceted defects are not energetically favorable.