Nextel™ 610 alumina fibers and alumina‐ YAG (yttrium‐aluminum garnet) matrices were used to make oxide‐oxide ceramic matrix composites ( CMC s) with and without monazite (La PO 4 ) fiber‐matrix interfaces. Twelve sequential aluminum oxychloride (Al OC l) infiltrations with 1 hour heat treatments at 1100°C and a final 1 hour heat treatment at 1200°C were used for matrix densification. This matrix processing sequence severely degraded CMC mechanical properties. CMC tensile strengths and interlaminar tensile ( ILT ) strengths were less than 10 MP a and 1 MP a, respectively. Axial fracture of Nextel™ 610 fibers was observed after ILT testing, highlighting the extreme degradation of fiber strength. Extensive characterization was done to attempt to determine the responsible degradation mechanisms. Changes in Nextel™ 610 fiber microstructure after CMC processing were characterized by optical microscopy, SEM , and extensively by TEM . In Al OC l degraded fibers, grain boundaries near the fiber surface were wetted with a glass that contained Y 2 O 3 /SiO 2 or Y 2 O 3 /La 2 O 3 /P 2 O 5 /SiO 2 , and near‐surface pores were partially filled with Al 2 O 3 . This glass must also contain some Al 2 O 3 and initially some chlorine. Al OC l decomposition products were predicted using the FactSage ® Thermochemical code, and were characterized by mass spectrometry. Effects of Al OC l precursors on monazite coated and uncoated Nextel™ 610 fibers tow and filament strength were evaluated. A mechanism for the severe degradation of the oxide‐oxide CMC s and Nextel™ 610 fibers that involves subcritical crack growth promoted by release of chlorine containing species during breakdown of intergranular glasses in an anhydrous environment is proposed.
No takes yet. Share an insight, caveat, or question.
Hay et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: