Normal incidence optical anisotropies are monitored during the growth of dielectric and metal films deposited at 45 degrees by logging the quantities R( perpendicular),R( ||), T( perpendicular) and T( ||) as functions of mass thickness d. For both ZrO(2) and Ti(2)O(3), the experimental profile of (R( perpendicular) - R( ||)) vs d is consistent with a refractive anisotropy that remains nearly constant during deposition. Gold, silver, and aluminum (deposited in the absence of oxygen) are shown to exhibit characteristic anisotropy vs d profiles that can be associated with the refractive index resonance in a globular metal film. The anisotropic effects observed in metals, both during deposition and during subsequent argon-ion sputter etching, are modeled by considering the film to comprise a mixture of crystallite-and void-defined materials and by adopting simplified structural hysteresis loops.
No takes yet. Share an insight, caveat, or question.
Ian J. Hodgkinson (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: