Time-resolved light scattering measurements were performed on gelation processes of poly(vinyl alcohol) (PVA) solutions at 25 °C in mixtures of dimethyl sulfoxide (DMSO) and water (H 2 O) with volume ratios of 60/40 and 80/20. It was found that the scattering profile I ( Q ) from a 60/40 (DMSO/H 2 O) solution has a maximum whose position Q m is independent of time and that the intensity I ( Q ) at Q = Q m increases exponentially with time. These observations agree with the theoretical predictions for the initial stage of spinodal decomposition (SD) type phase separation, while the scattering profile I ( Q ) from a 80/20 solution has no peak. It is therefore concluded that the SD type microphase separation occurs before gelation in the 60/40 solution, but not in the 80/20 solution. On the basis of present, as well as past results, a possible mechanism of the gelation process for PVA solutions has been proposed.
No takes yet. Share an insight, caveat, or question.
Takeshita et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: