The C 1s and O 1s X-ray absorption spectra of poly(ethylene terephthalate) (PET) have been recorded using transmission, fluorescence, and electron yield detection. The corresponding electron energy loss spectra (EELS) have been recorded in a scanning transmission electron microscope. These results are compared to the C 1s and O 1s spectra of gas phase 1,4-dimethyl terephthalate (the monomer of PET) recorded using EELS. The comparison of monomer and polymer materials in different phases and with different techniques has aided the understanding of the relative strengths and limitations of each technique as well as assisting the spectral interpretation. Good agreement is found in the overall shape and the energies of the spectral features. Relatively minor differences in intensities can be understood in terms of the properties of the individual spectroscopic techniques. The critical dose for radiation damage by 100 keV electrons incident on PET at 100 K is found to be (1.45 ± 0.15) × 10 3 eV nm -3 . In contrast, the critical dose for radiation damage by 302 eV X-rays incident on PET at 300 K is (1.2 ± 0.6) × 10 4 eV nm -3 . A figure of merit involving the product of critical energy dose and spectral efficiency (as expressed by the appropriate G value) is developed. This indicates that, for near-edge studies involving a 20 eV spectral width, there is ∼500-fold advantage of X-ray absorption studies on room temperature PET relative to electron energy loss studies of cooled PET.
No takes yet. Share an insight, caveat, or question.
Rightor et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: