Answers are grounded in this paper and cite their sources.
Various techniques for producing smooth clean silicon carbide substrates for use in epitaxial growth have been investigated. Three techniques stand out as being practical: a liquid etch containing 50% by weight KNO 3 in KOH which renders the (0001) face smooth when used at 600°C, thermal oxidation at 1200°C and above which results in smooth surfaces on both {0001} faces, and an anodic etch using HF solutions at room temperature which also results in two smooth faces but which can only be used satisfactorily on p-type material. The results obtained with these etches are discussed and techniques for using the electrolytic etch for junction delineation and improvement of diode characteristics are described.
No takes yet. Share an insight, caveat, or question.
Brander et al. (1967) studied this question.