Answers are grounded in this paper and cite their sources.
A range of cobalt catalysts, prepared using TiO 2 enwrapped with a hydrothermal carbon (HTC) layer, was used as a support for the Fischer–Tropsch synthesis (FTS). The effects of the HTC coating thickness and annealing process of HTC–TiO 2 on the structure and performance of the cobalt catalysts were investigated. The HTC coating with enrichment functional groups (e.g., COOH and COH) generated a strong interaction with the Co species during catalyst preparation and finally enhanced cobalt oxide dispersion. Furthermore, the protection of the surface of TiO 2 by a HTC coating improved the reducibility of the cobalt catalysts. The Co particle size was correlated with the thickness of HTC coating and the HTC–TiO 2 support annealing process. It was found that the HTC–TiO 2 support with a coating thickness of 8 nm and without an annealing process gave catalysts with a cobalt particle size of 8.6 nm and optimal FTS performance. The corresponding Co/8C-TiO 2 catalyst exhibited an activity 2.4 times higher than that of a Co/TiO 2 catalyst and showed 85% selectivity to C 5+ products under realistic FTS reaction conditions (210 °C, 1.0 MPa). The synergic effect of the HTC coating and the TiO 2 core had benefits on the catalytic properties of the Co/C-TiO 2 catalysts; the HTC coating improved dispersion and reducibility of cobalt species, while the existence of the TiO 2 core enhanced the stability of the catalyst structure in the reaction.
No takes yet. Share an insight, caveat, or question.
Liu et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: