Answers are grounded in this paper and cite their sources.
The roughness of the Si(100)/SiO2 interface is measured using both surface second harmonic generation (SSHG) and x-ray scattering. A comparison between these techniques shows a clear correlation for typical industrial oxides, despite the techniques being sensitive to differing regions of the roughness spectrum. The SSHG measurements are made using ∼10 fs pulses centered at 850 nm and at 80 MHz repetition rate. The short pulses produce a similar signal to noise ratio as earlier measurements, but use much lower average power, thus avoiding possible artifacts such as sample heating.
No takes yet. Share an insight, caveat, or question.
Cundiff et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: