Answers are grounded in this paper and cite their sources.
A ferromagnetic Fe0.013 Pd0.987 single crystal was examined with the polarized-beam neutron-diffraction technique in a study of the distribution of the localized magnetization in the alloy. Intensities of all nineteen Bragg reflections out to sinθλ=0.90 ^-1 were measured at 4.2^∘{}K in a field of 14 kOe, yielding the magnetic form factor averaged over all atoms. These data are fitted to a linear combination of calculated $3d$ and $4d$ free-atom form factors, resulting in a moment of 0.050±0.006 μB of $3d$-like moment and 0.088±0.008 μB of $4d$-like moment per average atom. A Fourier inversion of the magnetic scattering amplitudes emphasizes the aspherical shape of the unpaired-electron distribution. The over-all EgT2g ratio is 0.39±{}0.02. The measured saturation magnetization of this alloy is 0.114±0.004 μB per atom at 4.2^∘{}K, which is considerably smaller than the total moment of 0.138 μB seen by neutron diffraction. This discrepancy suggests a negative conduction-electron polarization of -0.024±0.011 μB per atom. The temperature dependence of the magnetic scattering amplitude and the saturation magnetization indicate that the conduction-electron polarization disappears near the Curie temperature, which is about 55^∘{}K. In addition, these data suggest that the $3d$ moment on an Fe atom and the $4d$ moments on surrounding Pd atoms are strongly coupled, although the range of the Pd polarization is not determined. The total d moment associated with the moment cluster around each impurity site is 10.7±0.6 μB.
No takes yet. Share an insight, caveat, or question.
Walter C. Phillips (1965) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: