Answers are grounded in this paper and cite their sources.
The Cr 3+ -doped K 0.6 (Mg 0.3 Sc 0.7 ) 2 (MoO 4 ) 3 crystal was grown from a flux of K 2 Mo 3 O 10 by the top seeded solution growth method. The K 0.6 (Mg 0.3 Sc 0.7 ) 2 (MoO 4 ) 3 crystal crystallizes in the rhombohedral system in space group R 3 c̅ . The K 0.6 (Mg 0.3 Sc 0.7 ) 2 (MoO 4 ) 3 crystal has a highly disordered structure. Investigation of the spectral properties of the Cr 3+:K 0.6 (Mg 0.3 Sc 0.7 ) 2 (MoO 4 ) 3 crystal shows that it exhibits broad absorption and emission bands, which are caused by the disordered structure of the K 0.6 (Mg 0.3 Sc 0.7 ) 2 (MoO 4 ) 3 crystal, except for the broad emission of Cr 3+ ions. On the basis of the absorption and emission spectra, the crystal field strength Dq/ B and Racah parameter C have been calculated. The Dq/ B value of 2.18 implies that Cr 3+ ion occupies the low crystal field site in the Cr 3+:K 0.6 (Mg 0.3 Sc 0.7 ) 2 (MoO 4 ) 3 crystal. These results suggest that the Cr 3+:K 0.6 (Mg 0.3 Sc 0.7 ) 2 (MoO 4 ) 3 crystal is a potential tunable laser crystal material.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: