Answers are grounded in this paper and cite their sources.
Electrical transport measurements have been made on p-type Hg1−xCdxTe with carrier concentrations ranging from 4×1015 to 1×1017 cm−3 and with x in the range 0.26–0.6. The acceptor ionization energy was determined to be about 14 meV by measurement of carrier freeze out in Hg0.6Cd0.4Te. Far-infrared photoconductivity and transmittance measurements in Hg0.6Cd0.4Te were used to verify this ionization energy of the acceptor. Calculations of both the ionized-impurity-scattering-limited mobility and the Hall coefficient as functions of temperature indicate that the p-type Hg1−xCdxTe crystals are compensated.
No takes yet. Share an insight, caveat, or question.
Scott et al. (1976) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: