This is the authors' abstract. We don't add key points for this paper.
We synthesized anisotropic Sm-Co and multi-layered Sm-Co/α-Fe nanocomposite thick-film magnets by post-annealing. The films were deposited on a Ta substrate at 200-300 °C, and then were post-annealed at 600 °C for magnetic hardening. The annealed Sm-Co films were mainly composed of SmCo5and had in-plane magnetic anisotropy. The magnetic anisotropy energy of the films was estimated from the in-plane and out-of-plane magnetization curves to be approximately 650 kJ/m3for the film deposited at 200 °C. Multi-layered Sm-Co/α-Fe films also exhibited anisotropic hysteresis loops and had coercivity of 250 kA/m. These results suggest that two-step annealing enables us to synthesize anisotropic Sm-Co/α-Fe thick nanocomposite films.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Furukawa et al. (2016) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: