Various zinc anodes with increasing calcium zincate (0%, 30%, 70%, 100%) were cycled at 50% theoretical Zn utilization to investigate cycle life and estimated cost. Failure mechanisms of majority 70% Zn/30% CaZn anodes are compared with pure CaZn.