The thermoelectric power (α) of p-type SnTe has been measured between room temperature and 450^∘{}C for apparent hole concentrations (p*=1eR₃₀₀) between 1×{}10²⁰ and 1.8×{}10²¹ cm^-3. At room temperature, α does not decrease monotonically with increasing p* in the usual manner for a p-type semiconductor. Instead, it increases from 5-8 {μ}V/deg at p*=1-2×10²⁰ cm^-3 to a maximum of 34{μ}V/deg at p*=8×10²⁰ cm^-3, after which it decreases to 20.5 {μ}V/deg at p*=1.8×10²¹ cm^-3. The maximum gradually disappears with increasing temperature. At 400 and 450^∘{}C, α decreases monotonically with increasing p*. By means of numerical calculations for a particular set of band parameters, it is shown that this type of anomalous variation in α can be exhibited by a p-type semiconductor with two nondegenerate valence bands. It is found that the observed properties of SnTe, including the variation of Hall coefficient with temperature and carrier concentration, are qualitatively consistent with a two-valence-band model, but are difficult to explain on the assumption that SnTe is a semimetal. However, it has not been possible to obtain a quantitative fit to the data with a two-band model in which both bands are of simple parabolic form.
No takes yet. Share an insight, caveat, or question.
Brebrick et al. (1963) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: