We have synthesized hierarchically porous Y 3 Al 5 O 12 (YAG) ceramics doped with trivalent cerium (Ce 3+ ) ions (YAG:Ce) by the sol–gel process and examined their optical properties including scattering strength. Starting from the ionic precursors, i.e., AlCl 3 ·6H 2 O, YCl 3 ·6H 2 O, CeCl 3 ·7H 2 O, and poly(ethylene oxide) (PEO) dissolved in a mixture of water and ethanol, monolithic wet gels are synthesized using propylene oxide as a geletion initiator. PEO induces phase separation parallel to the gelation in the sol–gel system to form bicontinuous morphologies consisting of gel- and fluid-phases. The wet gels thus obtained are subjected to either evaporative or supercritical drying, and then heat-treated to crystallize the gel skeletons to form YAG phase. The drying process critically affects the nanostructures of YAG skeletons after heat treatment; the supercritical drying results in skeletons consisting of fine grains (<50 nm), while evaporative drying yields skeletons with larger grains. The scattering strength of the heat-treated samples is evaluated by using coherent backscattering measurements and scattering-based hole burning, both of which clarify that the samples prepared via evaporative drying scatter visible light much more strongly than that prepared via supercritical drying.
No takes yet. Share an insight, caveat, or question.
Murai et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: