The purpose of this study was to compare the micro-tensile bond strength (µTBS) of three resin core composites to dentin and to examine the bonded interface of the composites. One experimental TDK-03(TD) and, two commercial, DC core Automix One (DC) and Unifil core EM(UN) were used. Flat dentin surfaces of human molars were exposed using #600 SiC paper and bonded with the respective adhesive of each system. After bonding, the composites were built up on the surfaces and cured under two conditions: "light condition" or "dark condition". µTBSs (MPa) in the light condition were: TD; 60.02±17.08, DC; 38.21±13.70, and UN; 29.50±9.71; in the dark condition: TD; 54.62±17.11, DC; 8.40±4.81, and UN; 9.47±6.56. Dark curing negatively affected the bond strength of the two commercial resin-core materials. The experimental material was not affected by the curing conditions.
No takes yet. Share an insight, caveat, or question.
Kadowaki et al. (2016) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: