Rod-form single crystals of Fe-19.43% Cr alloy of the bcc type about 3 mm in diameter and 12 cm in length were prepared. The thermal expansion and Young’s modulus in the temperature range −150°C to 250°C and the rigidity modulus at 20°C of the alloy were measured by means of a dilatometer, a vibrator-controlled oscillator system and the torsion pendulum method, respectively. The results of calculations based on the measured values have shown that the Young’s moduli of the single crystals at 20°C in the 〈100〉, 〈110〉 and 〈111〉 directions are 14.22×105, 22.23×105 and 27.37×105 kg/cm2, and the rigidity moduli at 20°C are 11.36×105, 7.21×105 and 6.43×105 kg/cm2, respectively ; the elastic anisotropy is not very large in all cases. The Young’s modulus in the 〈111〉 shows a small minimum at 10°C and a small maximum at about 110°C with increasing temperature, while the Young’s moduli in the 〈100〉 and 〈110〉 directions monotonously decrease. The mean temperature coefficients of Young’s modulus at 10°∼110°C are −32.77×10−5, −9.85×10−5 and +4.71×10−5 in the 〈100〉, 〈110〉 and 〈111〉 directions, respectively. The calculated value of Young’s modulus for the polycrystal agrees fairly well with the measured value for the polycrystal specimen prepared by melting.
No takes yet. Share an insight, caveat, or question.
Masumoto et al. (1971) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: