Demonstrates plasma chemical vapor deposition of amorphous aluminum nitride using trimethylaluminum, indicating characteristic material properties despite lacking crystalline structure.
AlN films have been successfully deposited by plasma CVD for the first time. Al was supplied by trimethyl Al (TMA) with H2 or N2 carrier gas, and N was supplied as NH3 through separate gas lines. The deposition rate depends upon the TMA supply, and is essentially independent of the NH3 flow rate. The composition of the deposited films was almost AlN, although a small amount of oxygen was always detected. A better film was obtained for the H2 carrier gas than for N2 carrier gas. X-ray diffraction profiles of the deposited films exhibited no crystalline AlN diffracting peaks, suggesting that the films are not crystallized, but the infrared and ultraviolet absorption spectra exhibited the presence of the Al–N bond (650/cm) and an optical band gap of 5.55 eV. The refractive index was about 1.9. These results suggest that the plasma-deposited films possess dominant AlN properties even though they are not crystalline.
No takes yet. Share an insight, caveat, or question.
Hasegawa et al. (1987) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: