Answers are grounded in this paper and cite their sources.
Propionic, n-butyric, isobutyric and phthalic acid esters of (hydroxypropyl)cellulose were prepared and characterized. The aliphatic esters were readily formed by reacting (hydroxypropyl)cellulose with the corresponding acid chloride at room temperature. The phthalic acid ester was formed by reacting phthalic anhydride with (hydroxypropyl)cellulose in pyridine at 45°C. The bulk aliphatic esters exhibit cholesteric reflection in the visible range of the spectrum. The wavelength of the reflection peak maximum, Λo, was measured spec-trophotometrically at different temperatures. Plots of Λº reached zero (i.e. the cholesteric pitch became infinite) at temperatures close to the anisotropic-isotropic phase transition temperatures. The latter temperatures were determined experimentally by polarizing micros-copy and differential scanning calorimetry, and were in the range 165°C ± 10°C for all cellulose derivatives studied in this work. The optical rotatory dispersion (ORD) and circular dichroism (CD) of thin layers of the planar cholesteric mesophase were also discussed.
No takes yet. Share an insight, caveat, or question.
Bhadani et al. (1983) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: