[ Co100-XZrX ] (x=10-40) alloys were prepared by using a mechanical alloying technique. Phase constitution of the crystallised material depended on the annealing temperature. The Co₈₂Zr₁₈ alloy crystallised at lower temperature around 550∘C consisted of Co₂₃Zr₆ , Co₅Zr and fcc-Co phases, while the alloy crystallised at higher temperature around 800∘C consisted of Co₂₃Zr₆ and fcc-Co phases. Phase constitution of the crystallised material also depended on the chemical composition of the alloy. The material with lower Zr content less than 10 at% Zr consisted of Co₂₃Zr₆ and fcc-Co, and the material with higher Zr-content over 30 at% consisted of Co₂Zr phase. The material containing 15-20 at% Zr consisted of Co₂₃Zr₆ , Co₅Zr and fcc-Co. Only the material containing Co₅Zr phase exhibited substantial coercivity, and it was confirmed that coercivity in the mechanically alloyed Co-Zr alloy was originated from the Co₅Zr phase.
No takes yet. Share an insight, caveat, or question.
Jeong et al. (2007) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: