Using radioactive tracer Fe‐59 and measuring rest activities after sectioning, the tracer diffusivities of Fe in almost single crystalline magnetite Fe 3‐Δ O 4 have been measured as a function of temperature and oxygen partial pressure. The measured curves log D Fe * /log p O2 all exhibit a minimum in the temperature range between 900°C and 1400°C in the homogeneity range of the magnetite. At sufficiently high oxygen partial pressures the slope ϱ log D Fe * /log p O2 is 2/3: at sufficiently low partial pressures it is —2/3. This allows to conclude that stoichiometric Fe 3 O 4 has a Frenkel disorder in the cationic sublattice, while at high oxygen potentials iron ion vacancies are responsible for the cation deficit. Their electrical charge is balanced by threevalent iron ions.