Answers are grounded in this paper and cite their sources.
In this study, three different types of hybrid structures SERS sensors made from different mixing ratio of trimetallic (Ag-Au-Pd) nanoparticles of [Au1: Ag1: Pd1] , [Au1: Ag2: Pd1] , [Au1: Ag2: Pd2] in surface alloying forms deposited on macro porous silicon (macroPsi) layer were created and extensively tested. By using a simple and fast immersion process, trimetallic (Ag-Au-Pd) nanoparticles were created utilizing ion reduction of numerous metallic salts on a macro porous silicon (macroPsi) layer. The macroPsi layers were created using a laser assisted etching (LAE) technique for 15 minutes with a constant density of approximately (28mA/c.m2). At a constant concentration (10-3 M) of HAu.Cl4, Ag.NO3 and Pd.Cl2 to synthesize Au-NPs, Ag-NPs and Pd-NPs, immersion processes with various mixing ratios were performed. The hybrid structures of SERS sensors were examined using XRD, FE-SEM, and Raman microscopes. The sensors were tested at different concentrations from 10-6 to 10-12 of MB target molecules. The SERS trimetallic sensors demonstrated a considerable reliance on hot spot zones among trimetallic nanoparticles. Higher enhancement factor with lower detection limit of Raman signal was obtained from [Au1: Ag2: Pd2] hybrid structures SERS sensor of about 1.5×1010 and 10-14 respectively, due to extra ordinary specific surface area and high surface density forming trimetallic nanoparticles . The variations of mixing ratio of trimetallic (Ag-Au-Pd) provide an effective pathway to develop the sensors performance towards detection of lower concentrations.
No takes yet. Share an insight, caveat, or question.
Shehab et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: