Answers are grounded in this paper and cite their sources.
Powders from HAF‐black/SBR mixtures in the total range of composition from 0 to 100% SBR were prepared by spray‐drying mixtures of aqueous dispersions of HAF‐black and SBR. Application of static pressure up to 19 kbar to these HAF‐black/SBR powders at room temperature yielded coherent specimens which in many respects behaved like vulcanized HAF/SBR compounds. The modulus‐pressure, modulus‐temperature, swelling and solubility behaviour of these systems was studied. The torsional modulus which was measured between −100 and +150 C showed an increase over several decades with increasing carbon‐black content. From the equilibrium swelling in toluene the apparent crosslink density of the polymer in the pressed HAF/SBR specimen was estimated. It was found that the apparent crosslink density increases with increasing carbon‐black content and also with the pressure at which the samples were prepared. The application of Vergnon's theory about the pressure dependence of the bulk modulus of metal powders to HAF‐black permitted to calculate the density of HAF‐black at ideal packing conditions as 2.00 g/cm3.
No takes yet. Share an insight, caveat, or question.
Schilling et al. (1974) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: