This is the authors' abstract. We don't add key points for this paper.
Kaolin has been identified as a potential raw material for the production of -Al 2 O 3 for hydrotreating catalyst support. This work explores the technical feasibility of applying the potassium hydroxide (KOH) extraction synthesis route on kaolin from the Belitung Island in Indonesia. The application of a published synthesis method to Belitung kaolin requires an approximately twofold increase in kaolin calcination time, an increase in kaolin calcination temperature from 950 to 1000 o C, and a tenfold increase in metakaolin extraction time, to obtain a specific surface area higher than 200 m 2 /g. The highest specific surface area of 233 m 2 /g was obtained when the kaolin was calcined at 1000 o C for 24 hours, and the metakaolin was extracted by concentrated KOH solution for 12 hours. Phase characterization of the final product confirmed the formation of -Al 2 O 3 , but with the inclusion of low-surface area -Al 2 O 3 phase.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Samadhi et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: