The aim of this study was to evaluate the healing of self-contained coronal defects on a sand-blasted, large-grit, acid-etched (SLA) surface implant, which had a calcium phosphate (CaP) coating applied by ion-beam-assisted deposition (IBAD). We also evaluated the effect of heating the coating to different temperatures. The CaP-coated SLA implants exhibited a slightly larger bone healing capacity in the self-contained coronal defect than SLA implants, indicating that combining SLA surface implants and a CaP coating by the IBAD method had synergistic effects on bone healing. There was no difference in the healing capacity between 350 degrees C and 450 degrees C heat treatment of the coating layer.