Thin films of tungsten oxide, titanium doped tungsten oxide and overlayers of titanium oxide/tungsten oxide have been produced by aerosol assisted CVD (AACVD) at 400 °C. The films were crystalline monoclinic WO3 by XRD, showing strong preferred orientation in the (0 2 0) plane. Films were blue on deposition (WO3−x; x ≈ 0.1). Fully oxidised yellow WO3 films were produced by annealing the blue films in air at 500 °C. The annealed films showed a photochromic transition to a coloured blue state when irradiated with 254 nm or 365 nm UV light. The colour change was reversible; the films returned to their original yellow colour when left in the dark, after which the blue colour could be regained by further UV irradiation. The WO3 and layered WO3/TiO2 films showed significant photochromism, while comparable thickness titanium doped WO3 films showed reduced photochromism, proportional to the level of Ti doping.
No takes yet. Share an insight, caveat, or question.
Palgrave et al. (2004) studied this question.
Synapse has enriched 3 closely related papers on similar clinical questions. Consider them for comparative context: