The authors evaluate the effect of different printing technologies (digital light processing [DLP], liquid crystal display [LCD]), and different printing angles (0°, 45°, 90°) on the mechanical (flexural strength [FS] and Vickers hardness number [VHN]) and chemical properties (degree of conversion [DC], surface microstructural, and glass transition temperature [Tg]) of a 3-dimension–printed denture base resin. Three-dimension–printed specimens (priZma 3D Bio Denture; MakertechLabs) were grouped: LCD0°, LCD45, LCD90°, DLP0°, DLP45°, and DLP90°. Thirty specimens were fabricated per group, for FS (12), VHN (12), DC (2), x-ray excited photoelectron spectroscopy (2), and Tg (2). For FS (MPa), a significant difference (SD) was found between DLP (93 [15]) and LCD (82 [14]) (2-way analysis of variance, P < .001), and 0° (79 ± 9), 45° (99 ± 12), and 90° (84 [16]) (Tukey test, P < .05). For VHN, no significant effects were detected (2-way analysis of variance, P >.05). Tg ranged from 80 °C through 100 °C for all groups. The highest means (SD) of DC were achieved for the specimens printed at 0° (DLP, 86.8 [3.7]%; LCD, 89.6 [0.3]%). The DLP system and 45° presented the highest FS, whereas the printing angle of 0° exhibited the highest DC. Considering that both systems (DLP, LCD) showed results above the threshold of 65 MPa for FS of denture base materials, and that LCD is a faster and lower-cost system, this technology could also be suggested for printing denture bases.
No takes yet. Share an insight, caveat, or question.
Viotto et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: