The evolution of phase and microstructure has been investigated for the spark plasma sintered anisotropic nanocrystalline SmCo6.1Si0.9 magnets. With the increasing of sintering temperature from room temperature to 680 °C, the phase evolves from 1:7H (TbCu7-type) single phase to 1:7H dominant phase plus 2:17 R (Th2Zn17-type) minor phase, and then to 2:17 R dominant phase with phase-transformation twins structure plus minor 1:5 H (CaCu5-type) precipitated phase with particulate morphology. The evolution of phase and microstructure in anisotropic nanocrystalline SmCo6.1Si0.9 alloys, as well as its effect on the coercivity is discussed and compared with that in nanostructured 2:17 type SmCo alloys.