Stress corrosion cracking (SCC) initiation in WE43 magnesium alloy exposed to simulated body fluid (SBF) at 37 °C was investigated using mechanism-based failure analysis . Microstructural characterisation, immersion corrosion testing, XPS, SEM/EDS and surface crack analysis were combined to identify features associated with crack initiation. The alloy contained rare-earth-rich intermetallic particles along grain boundaries and within the α-Mg matrix. These regions were frequently spatially associated with localised corrosion, pit formation and crack-damaged areas. Immersion testing showed an early transient corrosion response, with the corrosion rate decreasing from 2.1 mm y −1 at Day 1 to 0.31 mm y −1 at Day 28. However, mass loss and hydrogen evolution continued throughout exposure, indicating partial film protection rather than uniform passivation. Post-exposure cleaning revealed pits and trenches preferentially located near intermetallic-rich regions. XPS analysis identified a heterogeneous corrosion film containing Mg–O/Mg–OH species, P-rich Ca–P-containing products and trace chloride. This chemistry is consistent with non-uniform film protectiveness and local chloride-associated film destabilisation in SBF. Using the previously reported quasi-static SCC initiation threshold of 178 MPa as a mechanical reference boundary, SEM/EDS observations showed that SCC-type cracks were frequently associated with pits and RE/Zr-rich regions. The combined results support a pit-assisted SCC initiation sequence involving particle-associated localised corrosion, heterogeneous film stability, pit growth and pit-root stress concentration. Subsequent crack advance may involve dissolution-assisted processes, with possible hydrogen-assisted contribution requiring direct verification.
No takes yet. Share an insight, caveat, or question.
BHATT et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: