We report high room-temperature mobility in single-layer graphene grown by chemical vapor deposition (CVD) after wet transfer on SiO 2 and hexagonal boron nitride (hBN) encapsulation. By removing contaminations, trapped at the interfaces between single-crystal graphene and hBN, we achieve mobilities up to ∼70000 cm 2 V –1 s –1 at room temperature and ∼120 000 cm 2 V –1 s –1 at 9K. These are more than twice those of previous wet-transferred graphene and comparable to samples prepared by dry transfer. We also investigate the combined approach of thermal annealing and encapsulation in polycrystalline graphene, achieving room-temperature mobilities of ∼30 000 cm 2 V –1 s –1 . These results show that, with appropriate encapsulation and cleaning, room-temperature mobilities well above 10 000 cm 2 V –1 s –1 can be obtained in samples grown by CVD and transferred using a conventional, easily scalable PMMA-based wet approach.
No takes yet. Share an insight, caveat, or question.
Fazio et al. (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: