A relaxor ferroelectric ceramic for high energy storage applications based on 0.9BaTiO 3 –0.1Bi(Zn 0.5 Zr 0.5 )O 3 (0.9BT–0.1BZZ) was successfully fabricated via a conventional solid-state method.