A newly developed low Mn and high-Ca containing magnesium alloy, Mg-2.9Zn-1.1Ca-0.5 Mn (wt.%) based alloy was processed by low-temperature extrusion. The average recrystallized grain size decreased from 1.64 to 0.58 μm with a decrease in the extrusion speed from 1 to 0.01 mm s−1, but increased to 2.11 μm with increasing extrusion temperature from 270 to 350 ℃. The finest and uniform recrystallized grain structures with substantial nano-sized MgZn2 precipitates and α-Mn particles were obtained in the 270 ℃/0.01 mm s−1 sample. The texture intensity including basal (0002), prismatic type I (10−10) and prismatic type II (11–20) decreased accompanied by increasing the deformation temperature or extrusion speed. The weakest texture intensity for the 270 ℃/1 mm s−1 sample was derived from high degree of recrystallization, inhomogeneous recrystallized grain structure and the precipitates. Superior uniaxial tensile strength (yield strength of ∼352.5 MPa, ultimate tensile strength of ∼382.3 MPa and elongation of ∼7.1%) were achieved in the 270 ℃/0.01 mm s−1 sample. The improved yield strength was mainly ascribed to fine grain strengthening and precipitates strengthening relative to dislocation strengthening and back stress strengthening. A positive slope of work-hardening rate (dθ⁄dσ > 0) extruded at 270 ℃/0.01 mm s−1 was related to the sharp basal texture and insufficient slip. High θ value at stage IV after extrusion at 270 ℃/1 mm s−1 with abundant dimples and weak texture contributed to high ductility. Massive micro-cracks formed along the twins in the coarse deformed grains led to the failure during tension.
No takes yet. Share an insight, caveat, or question.
Nie et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: