Ten structurally different bisimide resins were prepared by reacting maleic anhydride/citraconic anhydride and benzophenone tetracarboxylic dianhydride with aromatic diamines and fused aromatic structures or heterocyclic groups. The amines included were 1,5‐diaminonaphthalene, 2,5‐bis(p‐aminophenyl)1,3,4‐oxadiazole, 3,3‐bis(p‐aminophenyl)phthalide, 9,9‐bis(p‐aminophenyl)fluorene. and 10,10‐bis(p‐aminophenyl)anthrone. These monomers were characterized by infrared (IR). 1H‐NMR, mass spectroscopy, and elemental analysis. Thermal polymerization of these monomers was investigated by differential scanning calorimetry. Broad exothermic peaks were observed for a temperature range of 225–380°C. Temperature of exothermic peak position was influenced by the presence of substituents at the olefinic bond, and in biscitraconimides it was 40–50°C lower than in the corresponding bismaleimides. Anaerobic char yields of cured bisimide resins ranged from 44 to 64%. Oxadiazole‐containing bisimides had low thermal stability. Increase in formula weight between the imide groups did not influence the char yields in a systematic manner. Graphite cloth laminates with two of these bisimide resins were fabricated and tested for a number of physical properties. Their limiting oxygen index was 70–72%.
No takes yet. Share an insight, caveat, or question.
Varma et al. (1982) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: