This is the authors' abstract. We don't add key points for this paper.
A simple method to directly convert Cs-exchanged IONSIV® IE-911 into a ceramic wasteform by hot isostatic pressing (1100 °C/190 MPa/2 hr) is presented. Two major Cs-containing phases, Cs2TiNb6O18 and Cs2ZrSi6O15, and a series of mixed oxides form. The microstructure and phase assemblage of the samples as a function of Cs content were examined using XRD, XRF, SEM and TEM/EDX. The chemical aqueous durability of the materials was investigated using the MCC-1 and PCT-B standard test methods. For HIPed Cs-IONSIV® samples, the MCC-1 normalised release rates of Cs were <1.57 × 10−1 g m−2 d−1 at 0–28 days, and <3.78 × 10−2 g m−2 d−1 for PCT-B at 7 days. The low rates are indicative of a safe long-term immobilisation matrix for Cs formed directly from spent IONSIV®. It was also demonstrated that the phase formation can be altered by adding Ti metal due to a controlled redox environment.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: