The purpose of this study was to explore the effects of changes in Type I collagen on the viscoelasticity of bone. Bone coupons were heated at either 100 or 200 degrees C to induce the thermal denaturation of Type I collagen. Half of these specimens were rehydrated after heat treatment; the other half were tested in a dry condition. The degree of denatured collagen (DC%) was analyzed by a selective digestion technique with the use of alpha-chymotrypsin. Isothermal (37 degrees C) and variable temperature tests (scans from 35 to 200 degrees C) were performed with the use of a dynamic mechanical analyzer to evaluate changes in bone viscoelastic properties as a function of collagen damage, specifically, changes in the loss factor (tan delta) and storage modulus (E') were assessed. Significant collagen denaturation occurred only when bone was heated at 200 degrees C irrespective of the hydration condition. Also, DC% did not show a significant effect on tan delta. However, higher values of tan delta were observed in wet samples compared to dry specimens. The temperature-scan tests revealed that the hydration condition, but not DC%, significantly affected the behavior of tan delta. However, E' was not strongly influenced either by DC% or by water content. These results suggest that at a constant frequency the denaturation of collagen triple-helical molecules may have few effects on the viscoelasticity of bone, but moisture may play a prominent role in determining this property.
No takes yet. Share an insight, caveat, or question.
Yamashita et al. (2002) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: