Poly(ethylene glycol)‐based networked polymers that had lithium sulfonate salt structures on the network were prepared by heating a mixture of poly(ethylene glycol) diglycidyl ether (PEGGE), poly(ethylene glycol) bis(3‐aminopropyl) terminated (PEGBA), and an ionic epoxy monomer, lithium 3‐glycidyloxypropanesulfonate (LiGPS). Flexible self‐standing networked polymer films showed high thermal stability, low crystallinity, low glass transition temperature, and good mechanical strength. The materials were ion conductive at room temperature even under a dry condition, although the ionic conductivity was rather low (10−6 to 10−5 S/m). The ionic conductivity increased with the increase in temperature to above 1 × 10−4 S/m at 90 °C. The film samples became swollen by immersing in propylene carbonate (PC) or PC solution of lithium bis(trifluoromethanesulfonyl)imide (LiTFSI). The samples swollen in PC showed higher ionic conductivity (ca.1 × 10−3 S/m at room temperature), and the samples swollen in LiTFSI/PC showed much higher ionic conductivity (nearly 1 S/m at room temperature).
No takes yet. Share an insight, caveat, or question.
Matsumoto et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: