Perovskite powders of La0.3Sr0.7CoO3–δwere prepared by the thermal decomposition of precursor complexes derived from nitrate solutions using ethylenediaminetetraacetic acid (EDTA) as a complexing agent. The calcination temperature is 920 °C. Powders thus obtained have a low carbon contamination. Dense ceramics with a relative density of about 96% have been prepared after sintering at 1150 °C.
No takes yet. Share an insight, caveat, or question.
Doorn et al. (1998) studied this question.