Luminescent K 2 ZrSi 3 O 9 (mineral wadeite): Ti with afterglow properties is reported for the first time. The structure analysis revealed that titanium ions were mainly substituted at the Zr 4+ sites of K 2 ZrSi 3 O 9 as the tetravalent state. The persistent luminescence peaks at 480 nm were strongly related to two factors, namely, charge transfer (CT) transition in a Ti-O polyhedron and oxygen vacancy around Zr 4+ sites. The K 2 ZrSi 3 O 9 wadeite including titanium ions is promising for application as a sensor using light energy storage materials.